Lo Pole Machine Cylinders Rehabilitation Methods Dec 07, 2016

1. wear increases the diameter of the barrel, if there is a certain amount of nitriding layer, directly within the cylinder bores, diameter of grinding to a new dimension, and then prepared according to the diameter of the new screw.

2. barrel inner diameter after machining trimming back casting alloys, thickness between 1~2mm and precision machined to size.

3. General cylinder wears out quickly, this section can be (take 5~7D long) boring dressing, coupled with a nitriding steel bushing diameter reference holes in the screw diameter, stay in the normal clearance, processing and preparation.